Table 1 Results of cellular uptake following overnight incubation of metal nanoparticles

From: Photon activated therapy (PAT) using monochromatic Synchrotron x-rays and iron oxide nanoparticles in a mouse tumor model: feasibility study of PAT for the treatment of superficial malignancy

  

Incubating Dose

Group

0.20 mg/ml

1.00 mg/ml

2.00 mg/ml

FeO NP (μg of Fe/106 cells)

30.7 ± 6.65

139.7 ± 16.30

168.8 ± 12.56

  1. 5 × 106 CT-26 cells were plated in each Petri dish containing different concentrations of MNP solution. Measured data are presented as the average uptake density per 106 cells in each incubating dose after harvesting cells for ICP measurements.